| Method | Precursors | Conditions | Products |
|---|---|---|---|
| Arc melting | Mn, Pt, Co | high-purity Ar | — |
Authors' explanation · Decomposed
The alloy decomposed into binary compounds.
Bounty Board › Permanent magnets › SBB-0119
Compiled from the literature and not yet reviewed by a curator. Suggest a correction
Ferrimagnetic all-d-metal Heusler from a high-throughput screen
Fully documented: a crystal structure, the prediction paper, the synthesis history and stability numbers.
Loading structure…
Predicted by Sanvito et al., Sci. Adv. 3, e1602241 (2017)
Regular Heusler ordering (Mn 8c, Co 4a, Pt 4b) built at the prediction paper's lattice parameter, then relaxed.
Sanvito et al. (2017) screened Heusler alloys in the AFLOW database with DFT and found Mn2PtCo to be one of 22 stable magnetic intermetallic Heuslers, with a ferrimagnetic ground state (1.13 μB/f.u.) and a formation enthalpy of -0.17 eV/atom, but within 30 meV/atom of its most favorable decomposition. Of the four predicted Heuslers the authors then tried to make, arc-melted Mn2PtCo decomposed into binary compounds.
| Property | Value | Method | Source |
|---|---|---|---|
| magnetic moment (ferrimagnetic ground state) | 1.13 μB/f.u. | DFT (AFLOW) | Sanvito et al., Sci. Adv. 3, e1602241 (2017) |
| formation enthalpy | -0.17 eV/atom | DFT (AFLOW) | Sanvito et al., Sci. Adv. 3, e1602241 (2017) |
| Method | Precursors | Conditions | Products |
|---|---|---|---|
| Arc melting | Mn, Pt, Co | high-purity Ar | — |
The alloy decomposed into binary compounds.
Tried to make it? Failed attempts are the most useful thing you can add. Report an attempt
Not yet documented.Suggest a route