Bounty Board › Batteries and ion conductors › SBB-0058
Compiled from the literature and not yet reviewed by a curator. Suggest a correction
Na10GeP2S12
Predicted 4.7 mS/cm Na conductor; the first synthesized sample reached only 0.012 mS/cm
- Status
- Claimed (partial)Made, but not yet with the predicted structure or property.
- Stability
- +10 at 27 °C+27 at 1000 °CmeV/atom; below zero is stable. Details
- Prediction
- 2015Cited 100 times
- Sponsor
- Sponsor wanted
On file: a crystal structure, the prediction paper and stability numbers. Missing: the synthesis history. Help fill it in
Candidate structure · P4_2/nmcfrom Alexandria
Loading structure…
Predicted by Kandagal et al., J. Mater. Chem. A 3, 12992 (2015); Richards et al., Nat. Commun. 7, 11009 (2016)
About this structure
Alexandria agm008882655. Checked against the prediction paper in the Nov 2026 structure review (P4_2/nmc (137) parent (LGPS type); ordered DFT models are lower symmetry, Li10GeP2S12 (LGPS) with Na on Li sites). Not yet confirmed: the review had medium confidence. The paper reports P4_2/nmc; the CIF is an ordered model in P1.
Why it matters
Kandagal et al. (2015) used ab initio molecular dynamics to predict that Na10GeP2S12, the sodium analogue of the Li10GeP2S12 superionic conductor, would conduct Na⁺ at about 4.7 mS/cm at room temperature with a 0.2 eV activation energy and a 2.7 eV band gap. Richards et al. (2016) computed 3.5 mS/cm and found it 7.2 meV/atom above the Na4GeS4 + Na3PS4 hull. Tsuji et al. (2018) first made a Na10GeP2S12 glass-ceramic by ball milling and heat treatment, with a structure similar to Na10SnP2S12, but it conducted only 1.2×10⁻⁵ S/cm at room temperature (activation energy 44 kJ/mol).
Predicted properties
| Property | Value | Method | Source |
|---|---|---|---|
| room-temperature Na-ion conductivity | 4.7 mS/cm | AIMD (extrapolated) | Kandagal et al., J. Mater. Chem. A 3, 12992 (2015) |
| activation energy (Arrhenius fit, 800–1400 K) | 0.2 eV | AIMD | Kandagal et al., J. Mater. Chem. A 3, 12992 (2015) |
| band gap | 2.7 eV | DFT | Kandagal et al., J. Mater. Chem. A 3, 12992 (2015) |
| room-temperature Na-ion conductivity (298 K) | 3.5 mS/cm | AIMD (extrapolated) | Richards et al., Nat. Commun. 7, 11009 (2016) |
Synthesis attempts
Known attempts (not yet entered as structured attempts): Na10GeP2S12 glass and glass-ceramic made by mechanical milling and subsequent heat treatment; the glass-ceramic phase resembles the tetragonal Na10SnP2S12 phase and conducts 1.2×10⁻⁵ S/cm at room temperature, activation energy 44 kJ/mol (Tsuji et al. 2018, ref attempt_glass; abstract read, precursors and temperatures not checked). No crystalline solid-state synthesis reaching the predicted conductivity was found. Searched Oct 23 2026.
Tried to make it? Failed attempts are the most useful thing you can add. Report an attempt
Proposed routes
Not yet documented.Suggest a route
References 3
- Prediction Kandagal et al., J. Mater. Chem. A 3, 12992 (2015). Theoretical prediction of a highly conducting solid electrolyte for sodium batteries: Na10GeP2S12
- Prediction Richards et al., Nat. Commun. 7, 11009 (2016). Design and synthesis of the superionic conductor Na10SnP2S12
- Experiment Tsuji et al., Chem. Lett. 47, 13 (2018). Preparation of Sodium Ion Conductive Na10GeP2S12 Glass-ceramic Electrolytes